professional factory for AISI 8620 Steel | 1.6523 | 21NiCrMo2 | SNCM220 Manufacturer in Argentina

professional factory for
 AISI 8620 Steel | 1.6523 | 21NiCrMo2 | SNCM220 Manufacturer in Argentina

Short Description:

AISI 8620 Steel is a low alloy nickel, chromium, molybdenum case hardening steel,generally supplied in the as rolled condition with a maximum hardness HB 255max. SAE steel 8620 offers high external strength and good internalstrength, making it highly wear resistant. AISI 8620 steel has a highercore strength than grades 8615 and 8617. SAE 8620 alloy steel isflexible during hardening treatments, thus enabling improvement ofcase/core properties. Pre hardened and tempered (uncarburized) 8620 ca...


  • Length: 3-5.8mm or Customization
  • Surface: black, peeled, or rough turned
  • Heat treatment: air-cooling, normalized, annealed, Q&T
  • Smelting process: EAF+LF+VD
  • Product Detail

    Product Tags

    Our products are widely recognized and trusted by users and can meet continuously developing economic and social needs for professional factory for AISI 8620 Steel | 1.6523 | 21NiCrMo2 | SNCM220 Manufacturer in Argentina, Create Values,Serving Customer!" is the aim we pursue. We sincerely hope that all customers will establish long term and mutually beneficial cooperation with us.If you wish to get more details about our company, Please contact with us now.


    AISI 8620 Steel

    is a low alloy nickel, chromium, molybdenum case hardening steel,
    generally supplied in the as rolled condition with a maximum hardness HB

    255max. SAE steel 8620 offers high external strength and good internal
    strength, making it highly wear resistant. AISI 8620 steel has a higher
    core strength than grades 8615 and 8617.

    SAE 8620 alloy steel is
    flexible during hardening treatments, thus enabling improvement of
    case/core properties. Pre hardened and tempered (uncarburized) 8620 can
    be further surface hardened by nitriding but will not respond
    satisfactorily to flame or induction hardening due to its low carbon
    content.

    Steel 8620 is suited for applications which require a
    combination of toughness and wear resistance. This grade is commonly
    supplied in round bar.

    1. AISI 8620 Steel Supply Range

    8620 Round Bar: diameter 80mm – 1200mm
    8620 Steel Plate: thickness 10mm – 1500mm x width 200mm – 3000mm
    8620 Square Bar: 140mm – 460mm
    8620 tubes are also available against your detailed request.
    Surface Finish: Black, Rough Machined, Turned or as per given requirements.

    2. SAE 8620 Steel Specification and Relevant Standards

    Country

    USA DIN BS BS

    Japan

    Standard

    ASTM A29 DIN 1654 EN 10084

    BS 970

    JIS G4103

    Grades

    8620

    1.6523/
    21NiCrMo2

    1.6523/
    20NiCrMo2-2

    805M20

    SNCM220

    3. ASTM 8620 Steels & Equilvalents Chemical Composition

    Standard Grade C Mn P S Si Ni Cr Mo
    ASTM A29 8620 0.18-0.23 0.7-0.9 0.035 0.040 0.15-0.35 0.4-0.7 0.4-0.6 0.15-0.25
    DIN 1654 1.6523/
    21NiCrMo2
    0.17-0.23 0.65-0.95 0.035 0.035 ≦0.40 0.4-0.7 0.4-0.7 0.15-0.25
    EN 10084 1.6523/
    20NiCrMo2-2
    0.17-0.23 0.65-0.95 0.025 0.035 ≦0.40 0.4-0.7 0.35-0.70 0.15-0.25
    JIS G4103 SNCM220 0.17-0.23 0.6-0.9 0.030 0.030 0.15-0.35 0.4-0.7 0.4-0.65 0.15-0.3
    BS 970 805M20 0.17-0.23 0.6-0.95 0.040 0.050 0.1-0.4 0.35-0.75 0.35-0.65 0.15-0.25

    4. AISI 8620 Steel Mechanical Properties

    • 8620 Physical Properties:

    Density (lb / cu. in.) 0.283
    Specific Gravity 7.8
    Specific Heat (Btu/lb/Deg F – [32-212 Deg F]) 0.1
    Melting Point (Deg F) 2600
    Thermal Conductivity 26
    Mean Coeff Thermal Expansion 6.6
    Modulus of Elasticity Tension 31

    • 8620 Steel Mechanical Properties

    Properties Metric Imperial
    Tensile strength 530 MPa 76900 psi
    Yield strength 385 MPa 55800 psi
    Elastic modulus 190-210 GPa 27557-30458 ksi
    Bulk modulus (typical for steel) 140 GPa 20300 ksi
    Shear modulus (typical for steel) 80 GPa 11600 ksi
    Poisson’s ratio 0.27-0.30 0.27-0.30
    Izod Impact 115 J 84.8 ft.lb
    Hardness, Brinell 149 149
    Hardness, Knoop (converted from Brinell hardness) 169 169
    Hardness, Rockwell B (converted from Brinell hardness) 80 80
    Hardness, Vickers (converted from Brinell hardness) 155 155
    Machinability (hot rolled and cold drawn, based on 100 machinability for AISI 1212 steel) 65 65

    5. Forging of Material 8620 Steel

    AISI

    8620 alloy steel is forged at a start temperature of around 2250ºF
    (1230ºC) down to approximately 1700ºF(925ºC.) prior to the hardening
    heat treatment or carburizing. The alloy is air cooled after forging.

    6. ASTM 8620 Steel Heat Treatment

    • Annealing

    AISI

    8620 steel may be given a full anneal by heat to 820℃ – 850℃, and hold
    until temperature is uniform throughout the section and cool in furnace
    or air cooled.

    • Tempering

    Tempering

    of heat treated and water quenched parts of 8620 steels (not
    carburized) is done at 400 F to 1300 F to improve case toughness with
    minimal effect on its hardness. This will also reduce the possibility of

    grinding cracks.

    • Hardening

    The

    AISI steel 8620 will be austenitized at around 840°C – 870°C, and oil
    or water quenched depending upon section size and intricacy. Cool in Air

    or Oil required.

    • Normalizing

    1675ºF

    (910ºC) and air cool. This is another method of improving machinability

    in 8620 material; normalizing might also be used prior to case
    hardening.

    7. Machinability of SAE 8620 Steel

    The

    8620 alloy steel is readily machined after heat treatment and/or
    carburizing, should be at a minimum so as not to impair the hardened
    case of the part. Machining may be done by conventional means prior to
    heat treatment – after carburizing machining is usually limited to
    grinding.

    8. Welding of 8620 Materials

    The
    alloy 8620 may be welded as rolled condition by conventional methods,
    usually gas or arc welding. Preheating at 400 F is beneficial and
    subsequent heating after welding is recommended – consult the approved
    weld procedure for the method used. However, welding in the case
    hardened or through hardened condition is not recommended

    9. Application of ASTM 8620 Steel

    AISI

    8620 steel material is used extensively by all industry sectors for
    light to medium stressed components and shafts requiring high surface
    wear resistance with reasonable core strength and impact properties.

    Typical

    applications are: Arbors, Bearings, Bushings, Cam Shafts, Differential
    Pinions, Guide Pins, King Pins, Pistons Pins, Gears, Splined Shafts,
    Ratchets, Sleeves and other applications where it is helpful to have a
    steel that can be readily machined and carburized to controlled case
    depths.

  • Previous:
  • Next:



  • A company whose principal activities consist of exploration for mineral, oil or gas may not progress to the next stage of development or to a stage where it is able to generate revenue. Other industry specific risks must also be considered.

    Zinc Markets, Exploration and Production (24 August 2015)
    Zinc ‘s many uses and potential supply deficit mean this mineral has high potential. What do investors need to know? The seminar will cover the risks and opportunities in zinc markets, exploration & production, including:
    Zinc and its uses
    Supply, demand and pricing
    Types and natural occurrence
    Exploration, Mining & Processing
    Opportunities and risks

    AMC Consultants is a leading independent mining consultancy, providing services exclusively to the minerals sector. AMC works with clients to plan new mines or improve the operations of existing mines, with a primary focus on achieving optimum output and return.

    Speaker
    MARK BERRY
    Principal Geologist, AMC Consultants
    Mark’s primary technical expertise is in mining geology, resource and reserve estimation, exploration and mining due diligence, geological risk management, expert reports, valuation, and training. His broad experience within the mining industry includes exploration, operations, project and financial management, stock/security exchange listing and compliance, research and development, and education. Mark’s experience encompasses base and precious metals, nickel, iron ore, coal, and industrial minerals.
    With over thirty five years’ of geology experience, focused on delivering innovative and high quality results within time and budget constraints, Mark is based in AMC’s Singapore office.

    Guest Panellist
    AZMAN JAAFAR
    Partner, RHTLawTaylorWessing
    Azman Jaafar is one of the founding members of RHTLaw Taylor Wessing and is the Head of the Firm’s Corporate Practice. His corporate practice focuses mainly on energy and resources, and hospitality industries. He has advised and represented clients in numerous transactions involving mergers and acquisitions, corporate finance, mining and oil and gas in Singapore, Indonesia, and the People’s Republic of China. Fluent in Mandarin and Bahasa Indonesia, he also heads the firm’s Indonesia Practice and manages the ASEAN Plus Group.



    Week three of the University of Edinburgh’s “Discovery of the Higgs Boson” (HIGGS) open online course.

    Prof Richard Ball
    School of Physics and Astronomy
    University of Edinburgh

    Licence: CC-BY-NC

    http://creativecommons.org/licenses/by-nc-sa/3.0/

    Send your message to us:

    INQUIRY NOW
    • * CAPTCHA: Please select the Car

    Related Products

    INQUIRY NOW
    • * CAPTCHA: Please select the Key