EN 34CrNiMo6 Steel is an important alloy engineering steel grade as per BS EN10083-3:2006. 34CrNim06 steel has high strength, high toughness and good hardenability. EN / DIN 34CrNiMo6 alloy steel has the stability ofresistance to overheating, but the white sensitivity of 34CrNiM06 ishigh. It also has the temper brittleness, so the weldability of34CrNiMo6 material is poor. The steel 34CrNiMo6 needs the hightemperature preheating before welding in order to eliminate the stressafter welding pr...


  • Length: 3-5.8mm or Customization
  • Surface: black, peeled, or rough turned
  • Heat treatment: air-cooling, normalized, annealed, Q&T
  • Smelting process: EAF+LF+VD
  • Product Detail

    Product Tags

    We stick to our enterprise spirit of "Quality, Efficiency, Innovation and Integrity". We aim to create more value for our customers with our rich resources, advanced machinery, experienced workers and excellent services for 9 Years Factory EN DIN 34CrNiMo6 | 1.6582 | 4337 Engineering Steel Factory from French, Looking to the future, a long way to go, constantly striving to become the all staff with full enthusiasm, one hundred times the confidence and put our company built a beautiful environment, advanced products, quality first-class modern enterprise and work hard!


    EN 34CrNiMo6 Steel
    is an important alloy engineering steel grade as per BS EN
    10083-3:2006. 34CrNim06 steel has high strength, high toughness and good
    hardenability. EN / DIN 34CrNiMo6 alloy steel has the stability of
    resistance to overheating, but the white sensitivity of 34CrNiM06 is
    high. It also has the temper brittleness, so the weldability of
    34CrNiMo6 material is poor. The steel 34CrNiMo6 needs the high
    temperature preheating before welding in order to eliminate the stress
    after welding processing.

    1.EN Steel 34CrNiMo6 Supply Range

    Round Steel Bar Sizes: diameter 80mm – 1200mm
    Other steel shape and sizes available according to your requirements.

    Surface finish: Black, machined, peeled, turned or according to other customers’ pecial requirements.

    2.EN 34CrNiMo6 Steel Standards And Equivalents

    BS EN 10083 -3: 2006 34CrNiMo6 / 1.6582 ASTM A29: 2004 4337
    BS EN 10250 – 3: 2000

    3. EN/DIN 34CrNiMo6 Steel Chemical Composition Properties

    BS EN 10083 – 3:2006 34CrNiMo6
    /1.6582
    C Mn Si P S Cr Mo Ni
    0.30-0.38 0.5-0.8 0.40 max 0.025 max 0.035 max 1.3-1.7 0.15-0.30 1.3-1.7
    BS EN 10250-3:2000 C Mn Si P S Cr Mo Ni
    0.30-0.38 0.5-0.8 0.40 max 0.035 max 0.035 max 1.3-1.7 0.15-0.30 1.3-1.7
    ASTM A29: 2004 4337 C Mn Si P S Cr Mo Ni
    0.30-0.40 0.6-0.8 0.20-0.35 0.035 max 0.040 max 0.70-0.90 0.20-0.30 1.65-2.00

    4.Mechanical Properties of EN/DIN 34CrNiM06 / 1.6582 Alloy Steel

    Properties < 16 >16 – 40 >40 – 100 >100 – 160 >160 – 250
    Thickness t [mm] < 8 8<t<20 20<t<60 60<t<100 100<t<160
    Yield strength Re [N/mm²] min. 1000 min. 900 min. 800 min. 700 min. 600
    Tensile strength Rm [N/mm2] 1200 – 1400 1100 – 1300 1000 – 1200 900 – 1100 800 – 950
    Elongation A [%] min. 9 min. 10 min. 11 min. 12 min. 13
    Reduction of area Z [%] min. 40 min. 45 min. 50 min. 55 min. 55
    Toughness CVN [J] min. 35 min. 45 min. 45 min. 45 min. 45

    5.Heat Treatment of 34CrNiMo6 Engineering Steel

    Quenched and Tempered (Q+T) of 34CrNiMo6 Steel

    • Heat 34CrNiMo6 round steel slowly to the temperature of 850°C;

    • Soak at this hardening temperature quench in oil;

    • Temper as soon as 34CrNiMo6 steels reach room temperature.

    • Heat uniformly to the suitable temperature;

    • Withdraw from the furnace and cool in the air.

    • The usual tempering temperature is 600°C which depending on the actual requirements.

    6.Forging of DIN 34CrNiMo6 / 1.6582 Steel

    Hot forming temperature: 1100-900oC.

    7.Machinability of Steel 34CrNiMo6

    Machining
    is best done with this 1.6582 alloy steel in the annealed or normalized
    and tempered condition. It can be machined by all conventional methods.

    8.Welding

    The
    alloy materials can be fusion or resistance welded. Preheat and post
    heat weld procedures should be followed when welding this alloy by
    established methods.

    9.Application

    EN DIN
    34CrNiMo6 steel is used to make tools which demands good plasticity and
    high strength. It is usually selected to make the big size and important
    parts, such as heavy machinery axle,turbine shaft blade, high load of
    transmission parts, fasteners, crank shafts, gears, as well as heavily
    loaded parts for motor construction etc.

    Otai Steel is reliable to
    supply engineering 34CrNiMo6 steels / 1.6582 engineering alloy steels.
    Please tell us your detailed requirements and have the best offer soon.

  • Previous:
  • Next:



  • Foshan Jopar Machinery Co.,Ltd mainly manufacturing decorative and industrial high frequency steel tube welding machine.

    Production process: Uncoiler– Forming stage–Welding stage–Welded head grinding stage–Sizing stage–Automatic cut of stage–End- product frame

    Production capacity:1-10 m/min
    Welder type: Ultrasonic Welding machine
    Cutting stage: Metal saw cutting stage

    Material: Our pip making machine can make Stainless steel , Carbon steel , Copper , Iron, MS, GI,Aluminium etc

    Application: Mainly used for decoration, products, appliances stainless steel pipe and carbon steel (round tube, square tube, shaped tube) production.



    Citric acid can be bought from drugstore (they use it in jelly or such to adjust acidity) but it is very expensive there. Therefore Finnish rodders buy it from some agriculture-store. It is not expensive. Officially it is used as pigs obstruent! I dipped those parts in citric acid for overnight, next day brushed it with wirebrush and flushed it with water. Then again back to citric acid over night and wirebrushed + flushed it next day.
    Flushing is important, you’ll want to get all acid away, otherwise steel will turn to yellow.
    You can’t use this method on all parts because of hydrogen embrittlement. So no pedals, frames, brake drums, engine blocks or such to citric acid!!! And yeah, parts should be clean -I’ve cleaned ‘em with fuel- because grease will neutralize acid. Ratio was 3%
    Parts must be dried soon as you get them flushed, I quess you guys know why…

    Music on the background:
    Junior Brown; “Sugarfoot Rag”

    Possibilities to comment this video was removed because answers to most of those questions can be found from this description. Been copy-pasting that text above too many times…

    Also, too many people don’t seem to understand that there are other methods than just media/sand blasting…

    Send your message to us:

    INQUIRY NOW
    • * CAPTCHA: Please select the Car

    Related Products

    INQUIRY NOW
    • * CAPTCHA: Please select the Star